ISO 9001 · 14001 · 45001 certified · EGPC-registered
DIAGNOSTICSWELL INTEGRITY

Enhanced Pipe Detection Tool (EPDT)

Electromagnetic inspection of up to five concentric pipes in one run, with the tubing left in place.

Pipes per run
Up to 5
Tool OD
~2 in
Pipe OD range
2⅞–26 in
Conveyance
E-line, SL, CT
EPDT transmitter and receiver coils inside the concentric pipe strings
Transmitter and receiver coils inside the pipe strings

APPLICATIONS

Where it is applied

  • Corrosion surveysMetal loss in the tubing and each casing string, with the tubing in place
  • Outer casingsThe strings a caliper cannot reach
  • Integrity baselinesThe well stock ranked by remaining wall
  • Workover planningThe failed string identified before the rig arrives
  • Life extension and abandonmentBarrier condition confirmed
  • Time-lapse monitoringCorrosion rate from repeat surveys

THE QUESTION IT ANSWERS

How much metal is left on each string, without pulling the tubing?

Repair, abandon or keep producing: decided on measured wall thickness per pipe, not on guesswork.

When to run it

  • Integrity status unknown across an ageing well stock
  • Before a workover, a change of service or abandonment
  • Sustained annulus pressure, run with noise and temperature logs
  • Corrosion monitoring between integrity campaigns

HOW IT WORKS

A pulse, a decay, a thickness per pipe

  1. 1Pulse. The transmitter coil drives a current I₀ that builds a primary magnetic field B₀.
  2. 2Switch off. The current is cut and the primary field decays.
  3. 3Eddy currents. The decay induces eddy currents Iₑ in each pipe wall, which generate a secondary field.
  4. 4Measure the transient. Receiver coils record the secondary field as it decays with time.
  5. 5Read the decay. Its shape and speed depend on conductivity, magnetic permeability and wall thickness, so analysing it quantifies the thickness of each pipe.
  6. Transmitter size and transmitter–receiver spacing set the depth of investigation: short spacings favour the inner pipe, long spacings see the outer strings.
Primary field B0, eddy current Ie and source current I0 around the tool
Primary field B₀, eddy current Iₑ, source current I₀
Transient decay curves from the first, second and third pipe
Transient decay from the first, second and third pipe

WHAT YOU GET

Data output and field cases

EPDT log: main and repeat passes with collars and metal-loss readings
Main and repeat passes, with collars and metal-loss readings

Each run delivers a VDL for quality control, inverted thickness loss for the first, second and third pipe, and collar positions across the strings, with our engineers' interpretation and an action list.

CASE 1

Severe damage on the third pipe in several localized areas over a 125 ft interval, with metal loss from 27% to 0%. Main and repeat passes agree within 2%.

CASE 2

High-integrity log data with an excellent signal-to-noise ratio: 8.4% corrosion on the outer pipe picked up from the log.

Reading the log: a collar shows on the VDL as a 20% increase in calculated thickness.

Why operators run it

  • Checks many pipes at onceUp to five layers in one run
  • No need to pull tubingSaving time, cost and risk
  • Works in many conditionsEven through coating, corrosion or scale
  • Real-time feedbackViewed live while running
  • Slim toolAround 2 in OD, fits small spaces
  • Collars, shoes and anomaliesLocates joints and unusual spots, not only thickness
  • Safer well decisionsRepair, abandon or keep producing
  • Higher logging speedMore footage per day on the same job

Typical specifications

Tool
Tool OD~2 in
Length~3–4 m
Pipes measurableUp to 5 concentric pipes
Pipe OD range2⅞ in (smallest) to 26 in (largest)
Depth resolutionCollar detection within ~0.1–0.2 m
Operating temperature~350 °F (175 °C)
Operating pressure~20,000 psi (138 MPa)
ConveyanceE-line, slickline or coiled tubing
Conveyance by well deviation
DeviationConveyance
Below 60°Wireline
60° to 70°Roller stem
Above 70°Coiled tubing
HorizontalTractor

The logging system: surface panel, downhole telemetry or power module, and centralizers, roller stem or tractor selected on deviation. Typical values; each run is confirmed against the well.

WHERE IT FITS

Diagnose, decide, act, record

  1. DIAGNOSEEPDT with spectral noise and high-precision temperature logs
  2. DECIDEWell integrity management: repair, abandon or keep producing
  3. ACTWIT and SIT tests, patches and bismuth-alloy barriers
  4. RECORDResults in the WelliRS barrier register, so the next crew inherits evidence

WHY IT PAYS · PUBLISHED SOURCES

Integrity problems are common, and expensive to find late

16%

Metal loss located in 9⅝ in casing through tubing, with EM thickness and noise logs; rig-based tubing retrieval avoided before P&A.

UK, Premier Oil, 2018 · SPE-190888-MS

10–30%

Of mature-field wells carry sustained annulus pressure in published surveys, so screening pays.

Schulz et al., J Pet Explor Prod Technol, 2025

30–45%

Of active wells worldwide carry some integrity issue.

Yakoot et al., GUPCO and Suez University, JPEPT 2021

Name one well and one question.

We plan the run with you: conveyance, passes, and the interpretation you will receive.

Plan an EPDT survey